Reduced Flow Battery Capacity Fade from Mixed Redox-Active Organics Beyond the Rule of Mixtures
Publication information:
Kyumin Lee, Kiana Amini, and Michael J. Aziz. 2025. “Reduced Flow Battery Capacity Fade from Mixed Redox-Active Organics Beyond the Rule of Mixtures”. ACS Energy Letters